SS410 stainless steel
Also called: AISI 410, 1.4006, X12Cr13, SUS410, martensitic stainless, 410 stainless
SS410 is a martensitic stainless steel with about 12% chromium. Unlike 304, it can be hardened by heat treatment and is magnetic, but its corrosion resistance is lower. It is used for valve and pump parts, shafts, fasteners and cutting tools.
Quick facts
- Type
- Martensitic stainless steel
- Chromium
- About 11.5–13.5%
- Hardenable?
- Yes, by heat treatment
- Magnetic?
- Yes
- Corrosion resistance
- Moderate: lower than 304
- Typical hardened hardness
- Roughly 35–45 HRC depending on tempering
Equivalent grades
| Standard | Grade |
|---|---|
| AISI / ASTM | 410 (UNS S41000) |
| EN / DIN | 1.4006 (X12Cr13) |
| JIS | SUS410 |
Typical chemical composition
| Element | % |
|---|---|
| Carbon (C) | 0.08–0.15 |
| Chromium (Cr) | 11.5–13.5 |
| Manganese (Mn) | 1.0 max |
| Silicon (Si) | 1.0 max |
Heat treatment
- Hardening: about 950–1010 °C, quench in oil or air
- Tempering sets the final hardness and toughness; avoid the range around 400–550 °C, where toughness and corrosion resistance suffer
- Annealed for machining, then hardened
Typical uses
- Valve trims, stems and seats
- Pump shafts and impellers
- Fasteners and springs
- Steam and gas turbine parts
- Cutlery and surgical tools (420 has more carbon for sharper edges)
Need parts made in SS410 stainless steel?
Post your requirement free. Workshops that take your kind of work see it and get in touch. You only talk to the ones that fit.
Get startedRelated
Related job work
Machines
Questions
- Is SS410 magnetic?
- Yes. As a martensitic stainless steel it is magnetic in all conditions.
- SS410 or SS304?
- SS410 can be hardened and is stronger and more wear-resistant; SS304 resists corrosion much better and cannot be hardened. Choose by whether strength or corrosion matters more.
- Does SS410 rust?
- It resists mild corrosion, but less than 304 or 316, and can rust in wet or salty conditions, especially if poorly finished.
The figures on this page are typical values for guidance, written by Diemeco from standard engineering practice. They are not a specification: confirm grades and properties with the relevant standard or the supplier's mill test certificate, and tolerances with your workshop. Last checked 8 October 2026.