Mild steel IS 2062
Also called: MS plate, E250, E350, IS 2062 E250 BR, structural steel, ASTM A36, S275
IS 2062 is the Indian standard for hot-rolled structural steel, the everyday "MS" plate, sheet and section used in fabrication. The grade number (E250, E350, …) is the minimum yield strength in MPa; it is easy to cut, bend and weld.
Quick facts
- Type
- Hot-rolled structural (mild) steel
- Most used grade
- E250 (yield 250 MPa min)
- Higher strength
- E350, E410, E450
- Weldability
- Excellent
- Density
- 7.85 g/cm³ (a 1 m² plate weighs 7.85 kg per mm of thickness)
- Forms
- Plates, sheets, angles, channels, beams, flats
Grades and strength
| Grade | Yield strength (min) | Tensile strength (min) | Elongation (min) |
|---|---|---|---|
| E250 | 250 MPa | 410 MPa | 23% |
| E350 | 350 MPa | 490 MPa | 22% |
| E410 | 410 MPa | 540 MPa | 20% |
| E450 | 450 MPa | 570 MPa | 20% |
Yield strength is lower for thick plates; the standard gives values by thickness.
Quality letters: A, BR, B0, C
- A: no impact test
- BR: impact tested at room temperature
- B0: impact tested at 0 °C
- C: impact tested at −20 °C, for cold or shock conditions
- So "E250 BR" means 250 MPa yield, impact tested at room temperature
Closest equivalents
| Standard | Grade |
|---|---|
| ASTM (USA) | A36 is close to E250; A572 Gr 50 is close to E350 |
| EN 10025 (Europe) | S235 / S275 near E250; S355 near E350 |
Typical uses
- Fabricated frames, structures and sheds
- Machine bases, guards and covers
- Base plates, brackets and gussets
- Tanks and chutes (not pressure parts)
- Laser- and plasma-cut profiles
Working with it
- Cuts cleanly by laser, plasma, gas or shearing
- Bends easily on a press brake
- Welds by MIG, stick or SAW without preheating in usual thicknesses
- Needs painting, galvanising or powder coating against rust
Need parts made in Mild steel IS 2062?
Post your requirement free. Workshops that take your kind of work see it and get in touch. You only talk to the ones that fit.
Get startedRelated
Related job work
Questions
- What does E250 mean in IS 2062?
- It is the minimum yield strength: 250 MPa. E350 has 350 MPa, and so on.
- What is E250 BR?
- Grade E250 in quality BR, which means its toughness has been impact tested at room temperature.
- How much does an MS plate weigh?
- 7.85 kg per square metre for every millimetre of thickness. A 10 mm plate weighs about 78.5 kg per square metre. Use the steel weight calculator for other sizes.
- Is IS 2062 the same as ASTM A36?
- They are close: A36 has a minimum yield of 250 MPa like E250. Small differences in chemistry and testing exist, so state the standard you need.
The figures on this page are typical values for guidance, written by Diemeco from standard engineering practice. They are not a specification: confirm grades and properties with the relevant standard or the supplier's mill test certificate, and tolerances with your workshop. Last checked 8 October 2026.