Aluminium 6351

Also called: 6351, AA6351, HE30, H30, AlSi1MgMn, 6351-T6

Aluminium 6351 is a medium-strength aluminium–magnesium–silicon alloy, known in India by its old name HE30 (or H30). In the T6 temper it is stronger than 6063 and close to 6061 and 6082, machines well and takes anodising. It is widely stocked in India as bars, plates and extruded sections for machined parts, frames, structures and transport parts.

Quick facts

Old Indian name
HE30 / H30 (IS 733)
Type
Al–Mg–Si, heat treatable
Tensile strength
About 290–310 MPa in T6
Density
About 2.7 g/cm³
Machinability
Good in T6
Anodising
Good

Equivalent grades

StandardGrade
AA6351
IS 733 (old)HE30 / H30
EN (close)6082 (AlSi1MgMn)

Equivalents are close, not identical. Name the grade and standard on the drawing.

6351, 6061, 6063 or 6082?

6351606160636082
Strength (T6)Medium–highMedium–highLowerMedium–high
MachiningGoodGoodFair (gummy)Good
Extruding complex shapesFairFairExcellentFair
Common in India asBars, plates, sectionsBars and platesWindow and frame profilesBars and plates

Typical uses

  • Machined brackets, housings and fixtures
  • Structural sections and frames
  • Truck, bus and railway parts
  • Pneumatic cylinder bodies and manifolds

Need parts made in Aluminium 6351?

Post your requirement free. Workshops that take your kind of work see it and get in touch. You only talk to the ones that fit.

Get started

Related

Questions

Is HE30 the same as 6351?
Yes, HE30 (or H30) is the old Indian name for alloy 6351; it is also close to 6082.
Can 6351 replace 6061?
In most machined parts, yes; check the drawing if a specific standard is named.
Can 6351 be welded?
Yes, by TIG or MIG, but strength near the weld falls unless the part is heat treated again.

The figures on this page are typical values for guidance, written by Diemeco from standard engineering practice. They are not a specification: confirm grades and properties with the relevant standard or the supplier's mill test certificate, and tolerances with your workshop. Last checked 29 October 2026.